@phdthesis{Youssef2022, author = {Youssef, Almoatazbellah}, title = {Fabrication of Micro-Engineered Scaffolds for Biomedical Application}, doi = {10.25972/OPUS-23545}, url = {http://nbn-resolving.de/urn:nbn:de:bvb:20-opus-235457}, school = {Universit{\"a}t W{\"u}rzburg}, year = {2022}, abstract = {Thermoplastic polymers have a history of decades of safe and effective use in the clinic as implantable medical devices. In recent years additive manufacturing (AM) saw increased clinical interest for the fabrication of customizable and implantable medical devices and training models using the patients' own radiological data. However, approval from the various regulatory bodies remains a significant hurdle. A possible solution is to fabricate the AM scaffolds using materials and techniques with a clinical safety record, e.g. melt processing of polymers. Melt Electrowriting (MEW) is a novel, high resolution AM technique which uses thermoplastic polymers. MEW produces scaffolds with microscale fibers and precise fiber placement, allowing the control of the scaffold microarchitecture. Additionally, MEW can process medical-grade thermoplastic polymers, without the use of solvents paving the way for the production of medical devices for clinical applications. This pathway is investigated in this thesis, where the layout is designed to resemble the journey of a medical device produced via MEW from conception to early in vivo experiments. To do so, first, a brief history of the development of medical implants and the regenerative capability of the human body is given in Chapter 1. In Chapter 2, a review of the use of thermoplastic polymers in medicine, with a focus on poly(ε-caprolactone) (PCL), is illustrated, as this is the polymer used in the rest of the thesis. This review is followed by a comparison of the state of the art, regarding in vivo and clinical experiments, of three polymer melt AM technologies: melt-extrusion, selective laser sintering and MEW. The first two techniques already saw successful translation to the bedside, producing patient-specific, regulatory-approved AM implants. To follow in the footsteps of these two technologies, the MEW device parameters need to be optimized. The MEW process parameters and their interplay are further discussed in Chapter 3 focusing on the importance of a steady mass flow rate of the polymer during printing. MEW reaches a balance between polymer flow, the stabilizing electric field and moving collector to produce reproducible, high-resolution scaffolds. An imbalance creates phenomena like fiber pulsing or arcing which result in defective scaffolds and potential printer damage. Chapter 4 shows the use of X-ray microtomography (µCT) as a non-destructive method to characterize the pore-related features: total porosity and the pore size distribution. MEW scaffolds are three-dimensional (3D) constructs but have long been treated in the literature as two-dimensional (2D) ones and characterized mainly by microscopy, including stereo- and scanning electron microscopy, where pore size was simply reported as the distance between the fibers in a single layer. These methods, together with the trend of producing scaffolds with symmetrical pores in the 0/90° and 0/60/120° laydown patterns, disregarded the lateral connections between pores and the potential of MEW to be used for more complex 3D structures, mimicking the extracellular matrix. Here we characterized scaffolds in the aforementioned symmetrical laydown patterns, along with the more complex 0/45/90/135° and 0/30/60/90/120/150° ones. A 2D pore size estimation was done first using stereomicroscopy, followed by and compared to µCT scanning. The scaffolds with symmetrical laydown patterns resulted in the predominance of one pore size, while those with more complex patterns had a broader distribution, which could be better shown by µCT scans. Moreover, in the symmetrical scaffolds, the size of 3D pores was not able to reach the value of the fiber spacing due to a flattening effect of the scaffold, where the thickness of the scaffold was less than the fiber spacing, further restricting the pore size distribution in such scaffolds. This method could be used for quality assurance of fabricated scaffolds prior to use in in vitro or in vivo experiments and would be important for a clinical translation. Chapter 5 illustrates a proof of principle subcutaneous implantation in vivo experiment. MEW scaffolds were already featured in small animal in vivo experiments, but to date, no analysis of the foreign body reaction (FBR) to such implants was performed. FBR is an immune reaction to implanted foreign materials, including medical devices, aimed at protecting the host from potential adverse effects and can interfere with the function of some medical implants. Medical-grade PCL was used to melt electrowrite scaffolds with 50 and 60 µm fiber spacing for the 0/90° and 0/60/120° laydown patterns, respectively. These implants were implanted subcutaneously in immunocompetent, outbred mice, with appropriate controls, and explanted after 2, 4, 7 and 14 days. A thorough characterization of the scaffolds before implantation was done, followed by a full histopathological analysis of the FBR to the implants after excision. The scaffolds, irrespective of their pore geometry, induced an extensive FBR in the form of accumulation of foreign body giant cells around the fiber walls, in a manner that almost occluded available pore spaces with little to no neovascularization. This reaction was not induced by the material itself, as the same reaction failed to develop in the PCL solid film controls. A discussion of the results was given with special regard to the literature available on flat surgical meshes, as well as other hydrogel-based porous scaffolds with similar pore sizes. Finally, a general summary of the thesis in Chapter 6 recapitulates the most important points with a focus on future directions for MEW.}, language = {en} } @phdthesis{OliveiraAlvesPereira2022, author = {Oliveira Alves Pereira, Ana Rita}, title = {Modelling of Mesenchymal Stromal Cells Interactions within the Skeletal Niche}, doi = {10.25972/OPUS-26660}, url = {http://nbn-resolving.de/urn:nbn:de:bvb:20-opus-266603}, school = {Universit{\"a}t W{\"u}rzburg}, year = {2022}, abstract = {Mesenchymal stem/stromal cells (MSCs) are a rare subpopulation of cells first identified in bone marrow with the potential to proliferate in plastic-adherent colonies and to generate de novo bone marrow stroma and its environment upon serial transplantation to heterotopic anatomical sites. Given their multipotency and self renewal competence, MSCs are prime prospective candidates for most modern musculoskeletal-tissue engineering and regenerative medicine approaches. Still, their envisioned therapeutic use is being questioned with concerns regarding their definition, characterization and integrative functions in vivo. It is well established that microenvironmental cues such as the extracellular matrix (ECM)-chemistry, the mechanical environment and local cellular and/or paracrine interactions critically control MSCs behavior. Yet, most of the scientific knowledge regarding the biology and therapeutic effect of MSCs originates from mechanistic in vitro studies where microenvironmental cues are hardly addressed. Therefore, manifestable changes in cell proliferation behavior and multilineage differentiation potential might be triggered that eventually compromise the translation of results to clinics. This thesis aims to address the complexity of MSCs interactions within the skeletal niche microenvironment in order to provide alternative methods to bypass the current MSCs in vitro culture limitations. Firstly, the influence of ECM-chemistry on MSCs behavior in vitro was explored by means of decellularized human bone models here established. Basal or osteogenic tailored cell-derived decellularized 2D matrices (dECM), proved to be suitable culture substrates for MSCs expansion by providing close-to-native cell-ECM interactions. Moreover, quantified morphological shape changes suggested a material osteo supportive potential, further functionally validated by observable spontaneous mineralization of MSCs. Aiming to identify novel intrinsic ECM regulatory features specific to the skeletal niche, 3D decellularized human trabecular bone scaffolds (dBone) were additionally developed and comprehensively characterized. Remarkably, the MSCs cultured on dBone scaffolds exhibit upregulation of genes associated with stemness as well as niche-related protein expression advocating for the conservation of the na{\"i}ve MSCs phenotype. vi On the other hand, the effect of biomimetic mineralization on MSCs osteogenic lineage differentiation potential was further addressed by hydroxyapatite functionalization of type-I collagen in presence of magnesium. Mineralized scaffolds exhibited higher cell viability and a clear trend of osteogenic genes upregulation comparing with non-mineralized scaffolds. Lastly, in order to mimic the complexity of the native MSCs environment, a dynamic culture system was applied to the 3D decellularized bone constructs, previously studied in single static conditions. Mechanical stimuli generated by (1) continuous perfusion of cell culture medium at 1.7 mL/min and (2) compressive stress from 10\% uniaxial load at 1 Hz, resulted in an improved cell repopulation within the scaffold and boosting of de novo ECM production. The stress-induced gene expression pattern suggested early MSCs commitment towards the osteogenic lineage mediated by integrin matrix adhesion, therefore further corroborating the recapitulation of a reliable in vitro bone niche model in dBone scaffolds. To conclude, the here developed in vitro models provide a progressive increased biomimicking complexity through which significant insights regarding MSC interactions with microenvironmental features in the skeletal niche can be obtained, thus surely paving the way for a better understanding of the role of MSCs in bone homeostasis and regeneration.}, language = {en} }