Molecular beam epitaxially grown short period (001) Hg\(_{1_x}\)Cd\(_x\)Te-HgTe superlattices have been systematically investigated. Several narrow well widths were chosen, e.g., 30, 35 and 40 Å, and the barrier widths were varied between 24 and 90 Å for a particular well width. Both the well width and the total period were determined directly by means of x-ray diffraction. The well width was determined by exploiting the high reflectivity from HgTe and the low reflectivity from CdTe for the (002) Bragg reflection. Knowing the well and barrier widths we have been able to set an upper limit on the average Cd concentration of the barriers, \(\overline x_b\), by annealing several superlattices and then measuring the composition of the resulting alloy. \(\overline x_b\) was shown to decrease exponentially with decreasing barrier width. The structure of a very short period superlattice, i.e., 31.4 Å, was also investigated by transmission electron microscopy, corroborating the x-ray diffraction results.
We have investigated oxygen on CdTe substrates by means of x-ray photoelectron spectroscopy (XPS) and reflection high-energy electron diffraction (RHEED). A Te oxide layer that was at least 15 A thick was found on the surface of as-delivered CdTe substrates that were mechanically polished. This oxide is not easily evaporated at temperatures lower than 350°C. Furthermore, heating in air, which further oxidizes the CdTe layer, should be avoided. Etching with HCI acid (15% HCl) for at least 20 s and then rinsing with de-ionized water reduces the Te oxide layer on the surface down to 4% of a monoatomic layer. However, according to XPS measurements of the 0 Is peak, 20%-30% of a monoatomic layer of oxygen remains on the surface, which can be eliminated by heating at temperatures ranging between 300 and 340 cC. The RHEED patterns for a molecular beam epitaxially (MBE)-grown CdTe film on a (lOO) CdTe substrate with approximately one monoatomic layer of oxidized Te on the surface lose the characteristics of the normal RHEED pattems for a MBE-grown CdTe film on an oxygen-free CdTe substrate.
We have grown HgTe/CdTe superlattices by molecular beam epitaxy; barrier thicknesses were in the range from 15 to 91 Å and the well thickness was maintained at a constant value of 30 Å. The infrared photoluminescence was investigated by means of Fourier transform infrared spectroscopy in the temperature range from 4.2 to 300 K. All superlattices showed pronounced photoluminescence at temperatures up to 300 K. To gain more detailed insight into the band structure of the HgTe/CdTe superlattices, band structure calculations were performed. The concept of the envelope function approximation was followed. Employing the transfer matrix method, the calculations were completed taking into account an eight band k·p model. An important parameter in these calculations is the natural valence band offset (VBO) between the well and barrier materials. As a general trend, the value for the direct gap decreases with increasing VBO. The experimentally determined energies of the band gap are in reasonable agreement with the values obtained by the theoretical calculations. A comparison between theory and experiment shows that the observed transition energies are closer to calculations employing a large offset (350 meV) as opposed to a small VBO (40 meV).
A semiempirical model is presented that correlates the broadening of the absorption edge with both transitions below the energy gap and with transitions by the Kane band model. This model correctly fits both the absorption and luminescence spectra of narrow-gap (Hg,Cd)Te samples that have been grown by the traveling heater method as well as by molecular-beam epitaxy. The accuracy of the band-gap determination is enhanced by this model.
We report on the growth of the compound semiconductor MgTe as weil as the ternary alloy Cd\(_{l-x}\)Mg, Te by molecular hcam cpitaxy. This is to our knowkdgc thc first time that this material has heen grown by any epitaxial technique. Bulk MgTe, which is hygroscopic, has a band gap of 3.0 eV and crystallizcs usually in thc wurtzite structure. Pseudomorphic films were grown on zincblende Cd Te suhstrates for a MgTe thickness helow a critical layer thickncss of approximately 500 nm. In addition, Cd\(_{l_x}\),Mg\(_x\)Te epilayers were grown with a Mg concentration between 0 and 68%, which corresponds to a band gap betwcen 1.5 and 2.5 eV at room temperature. The crystalline quality of thc layers is comparabk to CdTc thin films as long as they are fully strained. The lauice constant of zincblende MgTe is slightly smaller than that of CdTe, and the lattice mismatch is as low as O.7%. In addition highly n-type CdMgTe layers were fabricatcd by hromine doping. The tunability of the band gap as weil as the rather good laUice match with CdTc makes the matcrial interesting for optoelectronic device applications for the entire visible range.
The selected area epitaxial overgrowth of narrow gap HgTe as well as wide gap CdTe and ZnTe on CdTe/GaAs substrates, which had been structured by dry etching techniques, has been investigated. A plasma etching process using a barrel reactor with CH\(_4\)-CH\(_2\) gases has been employed to prepare stripes with a width of about 1 μm with anisotropic as well as isotropic etching profiles. It has been found, that the selected area HgTe overgrowth takes place with a high local selectivity to the low index planes of the patterned surface. In contrast, the selected area overgrowth of the wide gap CdTe and ZnTe is controlled by anisotropic growth kinetics provided that the substrate temperature is not lower than 220°C and the starting surface consists of well developed low index crystallographic planes.
The structural properties of HgSe grown by molecular beam epitaxy (MBE) are investigated for different lattice mismatches to the substrate and various growth conditions. The growth rate is shown to depend strongly on the growth temperature above lOO°C as well as on the Hg/Se flux ratio. It has been found that the crystalline perfection and the electrical properties are mainly determined by the layer thickness, especially for the growth on highly lattice mismatched substrates. Changes in the surface morphology are related to growth parameters. Differences between the electrical behavior of MBE-grown and bulk HgSe are discussed. The electrical properties of HgSe contacts on p-ZnSe are investigated as a function of different annealing procedures.